Manikandan,

1)Qualify PQR as per ASME SEC IX  . Additionally  consider and comply to  (API RP 934 C) with  BM as    SA 387 GR.11 CL.2 with butt joint /PWHT 
2)Qualify PQR as per ASME SEC IX  . Additionally  consider and comply to  (API RP 934 C) with  BM as    SA 387 GR.11 CL.2 with  WOL of TYP 347  /PWHT
   For WOL follow process which you want to use FCAW/GMAW/SMAW  

These two WPS s shall satisfy  your production Welding as mentioned  in above  query 

Thanks and regards

Vishwas -IWE 
International Welding Engineer 



On Thursday, January 19, 2023 at 4:38:56 PM UTC+5:30 manikandan J wrote:
Dear Experts,

We have a Vessel with the following MOC.(API RP 934 C)

Material 1 : SA 387 GR.11 CL.2 + SA 240 GR.347 (3.2 mm Cladded) -80 MM

Material 2 : SA 387 GR.11 CL.2 - 25 mm

Requesting your Technical inputs for PQR establishment.

Regards,
Manikandan
KSA

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/690c7c0c-7f90-4d67-ab86-96d8bf1043c1n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...