Re: [MW:33895] Re: ASTM A53 Gr.B TYPE E equivalent in ASTM

ASTM A 53 is a Pipe material specification

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Thu, Jan 5, 2023 at 12:04 PM Vishwas Keskar Welding Manager WELDING <vvkeskar123@gmail.com> wrote:
Pl. prepare comparative statement in detail  for both the Materials of interest.
Consult Engineer - Design
Jointly discuss the service application of the component under fabrication for which you are intending to change the MOC and then decide the material selection .

Regards

Vishwas -IWE 
International Welding Engineer
 
On Thursday, January 5, 2023 at 9:33:30 AM UTC+5:30 Sami MERT wrote:
Dear All,

Is ASTM A53 Gr.B TYPE E equivalent properties with S275JR (EN 10217-1) ? Could we use it instead of ASTM A53 Gr.B TYPE E?

Best Regards

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b9c7a47d-885a-4e6a-bbc4-6f11afa99ad7n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNmySJbxQGxaauDfHGoyc2xRqVnhC3-t9giD7dMVT%3Dwbg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...