Ref ASME B31.1, 136.4.1

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Mon, Dec 27, 2021 at 12:56 PM Vishwas Keskar <vvkeskar123@gmail.com> wrote:
There are no any guidelines in Codes for NDT after or before PWHT.
For Gr 91 welding , it is now after PWHT only.
In General  , industry standard is  as below
1. For Alloy steel,  NDT is after PWHT .
2.For Carbon steel , NDT is done before PWHT.

regards
Vishwas



On Sun, 26 Dec 2021, 22:17 Hany Nabil, <eng.hanynabil20@gmail.com> wrote:
Dear Gents

For NDT for storage Tank the NDT before or after PWHT 

If after what is the reason to do NDT after PWHT 

Please send reference code 

Thanks 
Hany Nabil 




--


 Best Regards,

 Eng. Hany Nabil
 Senior QA / QC Welding Engineer
 Egypt Mobile: 002-01225622022


This message, including any attachments, may contain confidential and privileged information for the sole use of the intended recipient(s). Review, use, distribution or disclosure by others is strictly prohibited. If you are not the intended recipient, or authorised to receive information on behalf of the recipient, please contact the sender by reply email, and delete all copies of this message. While we have taken reasonable precautions to ensure that this message and any attachments are free from viruses, we cannot guarantee that they are virus free and accept no liability for any damage caused by this message or any attachments. Messages sent or received through our networks may be monitored to ensure compliance with the law, regulation and/or our policies.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP1YJmTqh_%2BHRruBG1kyfM4dj0siPi5HcEHsmPR%3D_FK__4QAwg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3OhL4x0rbg5fs2s%2B7YhbHj5yp1YJHYr7%2BUt%2B%3DQw17optg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNhd03%2BNpi_5Lncf_i7LJQi%2BvsgrFGGXMH%3Dgjm4LKb5pg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...