I suppose follow ISO 15156-2 Table B3 as below.
Thanks & Regards
J.Gerald Jayakumar
On Sunday, 12 December, 2021, 12:59:58 pm GMT+4, Chintan Raval <chintan51@gmail.com> wrote:
Dear Experts
-- For pressure vessel as per asme sec 8 div 1
Client specification is asking for HIC test on PQR as per NACE TM 0284 using test solution A.
How ever acceptance criteria not specified
Kindly advice which acceptance criteria is apicable in this case