Friday, December 3, 2021

Re: [MW:32632] DENSITY OF RT FILM

Worst area where IQI placed and Sensitivity achieved in that particular area
to 
Best area where IQI placed density check. 
where us densitiy range -15% to 30%

Thank you, 

Regards, 
S.SENTHILKUMAR


On Friday, 3 December, 2021, 08:44:07 am IST, SEN SEN <senins054@gmail.com> wrote:


Dear experts
    while doing film interpretation, which all area need to be checked for density with densitometer? spec says 1.8 to 3.5, is it only for weld area or also for entire area of film

please clarify with  which code,
thanks with regards,
senthil P

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGYkEe2ecsSUJVSKCTzo9H59mrMwKFSiMyNz87NHu9Gq3cL3sw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...