Re: [MW:32679] AWS WPS & WELDER QUALIFICATION

Don't write anything, it will confuse others.
It's not Asme sec IX we are talking about.

Refer AWS D1.1...position is essential variable...PQR in 3G position qualifying vertical position only.
2G qualify flat and horizontal 



On Sun, 12 Dec 2021, 11:50 Chandan Singh, <chandans985@gmail.com> wrote:
Hi,

Position is non essential, that's why not required addition WPS & PQR.


On Wed, Sep 1, 2021 at 5:20 PM DINESH KUMAR DEVENDHIRAN <dineshqc05@gmail.com> wrote:
Dear Experts
I need a clarification on AWS table 4.1 vs 4.10
As per table 4.1- for 3G position WPS shall be qualify for vertical position only
As per table 4.10 - for 3G position welder will qualify for Flat, Horizontal, vertical.

My doubt is if i have a WPS for 3G uphill position, can i use the same WPS for 1G&2G also ?
If not please explain.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/571704be-652c-417c-9c67-6400ec82034an%40googlegroups.com.


--
Regards
CHANDAN SINGH
Sterling & Wilson 
+919981575817
+917379619175


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BtZUbUEkFcN879PoNiKVoX-Gt7po2WbhhVuKamkAqFDh7mUOA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOenW4g_heGtvmfx9n%3DbmzKeM8TRMQ%3DsyT7wNDzqogdjBeUWfQ%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...