There is no particular software for PQR and WPS. You just need to follow the format mentioned in code either Asme Sec-ix or Api 1104.. 

On Sat, Dec 25, 2021, 9:44 AM Shahil Saini <sainishahil98@gmail.com> wrote:
Hello everyone, Hope you all are doing well

I want to know which software is used for preparation of WPS and PQR? And the software is easy to understand and free to use.

Thank you,

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALfBO_8955-kN9wgKjNRTCNQ2FdqaXrXdDjjb%3Ds-gDmkm74aKg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHqH7yD4uirOp3vn0i50JTkxUG_-FkUbee3MJGnHw5oPL%2BSKZA%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...