Friday, December 10, 2021

Re: [MW:32669] Hydrotest as per ASME B 31.3

Pressure Test and Leak test are two different tests; used for different purposes.

On Tue, 12 Oct 2021, 15:47 krishna kamal nayan Pandey, <kkmech1987@gmail.com> wrote:
Dear Experts,
As per b 31.3 Joints can be painted before leak test. Is the leak test referred here as a hydrotest also? Please confirm.


Best Regards,

 

Krishna Kamal Nayan  


 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN%2Bgo9BBYPf%2BLOCJ-S-7BfZDce_oxVfV1gqYpr7WKeg5m5eb%3Dg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOenW4h7PaYC3SJHnbWTZHc4MNzqTQ%2BRzf_Z-AJ-3D6cajTH2w%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...