Re: [MW:32688] Dissimilar material with impact test

Dear Mr. George

Thanks 
But I think impact test required on minimum tensile strength only.

Can you explain me which reference article in ASME B31.3

Thanks 
Hany Nabil
On Fri, Dec 17, 2021 at 7:10 AM George Dilintas <dilintas@gmail.com> wrote:
Impact test is applicable for weld metal and both heat affected zones. You follow B31.3 to the letter

Στις Τετ 15 Δεκ 2021 στις 5:16 π.μ., ο/η Hany Nabil <eng.hanynabil20@gmail.com> έγραψε:
Dear Gents

If we have WPS with two materials, P-1 to P-8 and impact test required,
According to ASME B31.3, we can apply impact test on one side only ( carbon steel) ?
Or shall be applying impact test on SS with CS ?

Please advise 


Thanks,

Hany Nabil
Welding Engineer 
--


 Best Regards,

 Eng. Hany Nabil
 Senior QA / QC Welding Engineer
 Egypt Mobile: 002-01225622022


This message, including any attachments, may contain confidential and privileged information for the sole use of the intended recipient(s). Review, use, distribution or disclosure by others is strictly prohibited. If you are not the intended recipient, or authorised to receive information on behalf of the recipient, please contact the sender by reply email, and delete all copies of this message. While we have taken reasonable precautions to ensure that this message and any attachments are free from viruses, we cannot guarantee that they are virus free and accept no liability for any damage caused by this message or any attachments. Messages sent or received through our networks may be monitored to ensure compliance with the law, regulation and/or our policies.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP1YJmRrDRHB-c2Y_cmmyN8A0B%3DMGqJ59g-SKdAtmc6ObptjAw%40mail.gmail.com.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40Be_NLenfpVmqp8z6ZLwtmjBseOZFjtFG_EzV%2BjRN%3DKHw%40mail.gmail.com.
--


 Best Regards,

 Eng. Hany Nabil
 Senior QA / QC Welding Engineer
 Egypt Mobile: 002-01225622022


This message, including any attachments, may contain confidential and privileged information for the sole use of the intended recipient(s). Review, use, distribution or disclosure by others is strictly prohibited. If you are not the intended recipient, or authorised to receive information on behalf of the recipient, please contact the sender by reply email, and delete all copies of this message. While we have taken reasonable precautions to ensure that this message and any attachments are free from viruses, we cannot guarantee that they are virus free and accept no liability for any damage caused by this message or any attachments. Messages sent or received through our networks may be monitored to ensure compliance with the law, regulation and/or our policies.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP1YJmRN%3DOoSVMpJVduH9utsqgDuagL_4TrNRv9Amwvt0ag4dg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...