Re: [MW:32639] NDT Requirements (Applicable CODE B31.3 )

Gap control check is done by RT.

On Tue, Dec 7, 2021 at 7:34 AM Chaudhary Zafar Iqbal <chzaiqbal88@gmail.com> wrote:
Dear Experts ,

Good Day,

Is it required as per B31.3 to do the RT for the fillet socket weld joints ?

we have done Penetrant Testing , is it enough ?

Best Regards,
Zafar 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP9k9Xety7w4tUPKr7Lz%2Bo1WCp6S0fJXDskWRm4cSwGv%3DoMjuQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFycdMzdaY3a59y%3DB1H8TkbL2dxZLDfNV1WOfBmrCSDcCucVPA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...