Monday, December 27, 2021

Re: [MW:32706] Dish End Spin Hole Block

Hole is accepted as per ASME sec viii. But you have to make "v" On hole and than patch. Also patch should be radiography examination.. 

Thanks & Regards
Sushil Gaur. 
M. No. 9530278378

On Sun, 26 Dec, 2021, 10:17 pm Rahul Chaudhari, <navyrahul@gmail.com> wrote:
Dear All, 
Greetings.

WE have manufactured 10% torispherical dish end in house & block dish ends spin hole as per attached photographs. 
Please kindly advise me, is it acceptable as per good engineering practice or not?
Material IS IS2062. Thickness is 10mm. Job - horizontal storage tank


Thanks & Regards,

Rahul Chaudhari
+918149199922

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHjJ0V9Dy0ZrYO60YQkbyXXwHaNkqB8AkXreW-ZM_fc75oqVBA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAKVvO9NPaf442Wsne3duyWVBV18V%3DBpeYZ7MUMqH4NKB_Y2Uw%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...