Sunday, December 26, 2021

Re: [MW:32703] Dish End Spin Hole Block

Dear Rahul,

Not acceptable

On Sun, Dec 26, 2021 at 5:47 PM Rahul Chaudhari <navyrahul@gmail.com> wrote:
Dear All, 
Greetings.

WE have manufactured 10% torispherical dish end in house & block dish ends spin hole as per attached photographs. 
Please kindly advise me, is it acceptable as per good engineering practice or not?
Material IS IS2062. Thickness is 10mm. Job - horizontal storage tank


Thanks & Regards,

Rahul Chaudhari
+918149199922

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHjJ0V9Dy0ZrYO60YQkbyXXwHaNkqB8AkXreW-ZM_fc75oqVBA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0yo2JsfJx5A7xLnnE1aRvsnq9tc4oLhf%2BHuMb3G579%2BMw%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...