Dear Experts ,

Can we using Stellite 21 cladding on top of SA 217 grade material ? Pls advise ur inputs

BR
Neilashkumar P 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/515293241.2676688.1640707430107%40mail.yahoo.com.

No comments:

[MW:35668] Selection of Filler/Electrode.