Friday, December 10, 2021

Re: [MW:32676] AWS WPS & WELDER QUALIFICATION

Hi,

Position is non essential, that's why not required addition WPS & PQR.


On Wed, Sep 1, 2021 at 5:20 PM DINESH KUMAR DEVENDHIRAN <dineshqc05@gmail.com> wrote:
Dear Experts
I need a clarification on AWS table 4.1 vs 4.10
As per table 4.1- for 3G position WPS shall be qualify for vertical position only
As per table 4.10 - for 3G position welder will qualify for Flat, Horizontal, vertical.

My doubt is if i have a WPS for 3G uphill position, can i use the same WPS for 1G&2G also ?
If not please explain.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/571704be-652c-417c-9c67-6400ec82034an%40googlegroups.com.


--
Regards
CHANDAN SINGH
Sterling & Wilson 
+919981575817
+917379619175


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BtZUbUEkFcN879PoNiKVoX-Gt7po2WbhhVuKamkAqFDh7mUOA%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...