Skip to main content

[MW:31992] Welding between api 5l X60 to AISI 4130

Dear All,
Refer to below mail there is small correction * low alloy steel 


On Sun, 14 Feb 2021 at 10:31, seejo nereparambil
<seejonj@yahoo.com> wrote:
Dear Experts,
We are in process of Proceedure qualification for CS to Low carbon steel. Hence ,i am seeking your advise to select suitable welding electrodes for  welding between AISI 4130 to API 5L X60 material
Design code is ASME B 31.3 and qualification in accordance with SecIX, thickness is 14.27 mm

Kindly provide your recommendation 

Rregards
Seejo



On Thu, 4 Feb 2021 at 11:38, sunil kaushik
<sunilkaushik08@gmail.com> wrote:
PMI is the sorting method .you shoul go for the wet analysis testing.

On Wed, 3 Feb, 2021, 9:17 am Pravin Poornachandran, <htcispravin@gmail.com> wrote:
Dear expert, 

Good day. 

Recently I performed WPS for ER70S-G for nace requirement project. 
Based on welding consumable mill certificate as per EN10204 3.1, Ni <1% and these chemical analysis is conducted in authorised laboratory following the method specified in industrial code. It is laborious procedure and accurate. 

But when we perform PMI, Ni values shows 1.2-1.5, which client is questioning now. 
I did contacted consumable supplier and they are very certain Ni is less than 1%. 

Can anyone advice how should I handle this situation. 

Best regards,
Pravin Poornachandran 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADDyn7cJnBBffbUGsDUJKPoFzVRvnQ-yOkMV89Ur_sGJiPcemQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAA-uzKWwCk1yNyUfbMRbMO8AJfdd8pce4XdnxfpetqJiLgHvTw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/833242771.1076565.1613288159630%40mail.yahoo.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...