Dear Nikhil ;We qualify for thickness range . Diameter is not essential
On Sat, 31 Oct 2020 at 12:25, NIKHIL THOMAS JOY <nikhil.thomasjoy@gmail.com> wrote:
Dear Experts,Greetings of the day.I have a doubt regarding the WPS preparation.I have prepared one PQR of GTAW+SMAW in P22 material of size 6 inch.But in wps the qualified diameter what I should write as per asme sec 9 , qw-200.Is this can qualified for all the diameter?Should i need to write any diameter range in wps.Even though the thickness range is 5 to 2T.Experts please advise me.--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6c9cd6e7-1d3d-426d-adb7-d361351c767an%40googlegroups.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29OiLfv%2BnU2jt1vHSxzPkQ8R-tfGHn2U-PmoSGKUk6q4wCQ%40mail.gmail.com.