Re: [MW:31615] POST HEATING IN PWHT


SA 335 grade P9- preheat given 200 degree only as per client requirement then once welding completed , preheat will be increased upto 350 for half an hour.

Rate of heating is same as pwht like 100 degree per hour.

Thanks & Regards
Chan

On Mon, 26 Oct 2020, 08:41 NIKHIL THOMAS JOY, <nikhil.thomasjoy@gmail.com> wrote:

Dear sir, Good evening

Sir, kindly please  solve my doubt related to POST HEATING IN PWHT.

1.Where we need to do post heating.

2.If I am doing pwht sudden after welding is there any need of post heating or not.

3.In any code post heating mentioned.

Please give me answer for the above mentioned question.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5d07c2d7-f780-459d-8aab-53e92469c23cn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGWOcnrzZSh7nxR%2BDZ7T-gE5-KYTN5yiNjGFr5We5EZTkPbHQg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...