Hi,

There is no problem, need  to do atleast  half thickness or hot pass which ever is greater before removing the clamp/before interruption of weld.

On Thu, 22 Oct 2020, 17:28 dorh, <dorrihriz@gmail.com> wrote:

Hello ;

We work for welding activity pipeline 12"         X52       thickness 8.38 mm

Root / hot pass      GTAW

Filling / cap            SMAW

In order to optimize production Contractor propose to proceed with GTAW  first ,   for example for he weld  first 10 weld joint GTAW  after that he come back tomorrow  with and filling and cap  weld joint with SMAW.

 

It's some issue for that    ?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/386e7357-4115-479b-b8bf-45df08b78becn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABGg_FJ2B6huL_sS%2BSpP9_Kd9Z5gn52W%2BwBn8CFkCC0%3DhjtrCQ%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...