Re: [MW:31596] welding activity pipeline

Dear Sir, Check your WPS whether it is single heat cycle or 60% of the thickness to be weld before welding going to stop, in our project min 60% to be weld shall be completed.
Thanks & Regards

On Thu, 22 Oct 2020, 20:26 Kannayeram Gnanapandithan, <kgpandithan@gmail.com> wrote:
check api 1104, time laps are important if you have specified in WPS

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Thu, Oct 22, 2020 at 5:28 PM dorh <dorrihriz@gmail.com> wrote:

Hello ;

We work for welding activity pipeline 12"         X52       thickness 8.38 mm

Root / hot pass      GTAW

Filling / cap            SMAW

In order to optimize production Contractor propose to proceed with GTAW  first ,   for example for he weld  first 10 weld joint GTAW  after that he come back tomorrow  with and filling and cap  weld joint with SMAW.

 

It's some issue for that    ?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/386e7357-4115-479b-b8bf-45df08b78becn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePzNafztur0Gku74he5vfSh%2ByffBzkvdf6%2BCrG3iLyurA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABQUuFgDwqcJ4%2BdyeQ214qAjysaLvTcaQb0KDMXYB2PDc2Gtww%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...