Re: [MW:31634] POST HEATING IN PWHT

You question is very general.

PWHT depends on the following factors:

Thickness
Material grade
Service requirements (example: lethal service)

For some grades (Pno-15E materials) preheat maintenance is required when PWHT is not done immediately after welding

Στις Δευ, 26 Οκτ 2020 στις 6:41 π.μ., ο/η NIKHIL THOMAS JOY <nikhil.thomasjoy@gmail.com> έγραψε:

Dear sir, Good evening

Sir, kindly please  solve my doubt related to POST HEATING IN PWHT.

1.Where we need to do post heating.

2.If I am doing pwht sudden after welding is there any need of post heating or not.

3.In any code post heating mentioned.

Please give me answer for the above mentioned question.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5d07c2d7-f780-459d-8aab-53e92469c23cn%40googlegroups.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40C3Y_W2mXKEnbcjZfmDZtnp3QcGJ2A3hfLu_Paanw2JQQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...