Re: [MW:31611] Re: WPS and PQR According to ASME Sec.IX and Sec.VIII- Boiler and Pressure Vessel Code

For your Welding procedures (WPS and the respective PQR) you must use ASME BPVC Section IX, but if your construction code is ASME BPVC Section VIII Div. 1 you must see in this Code the preheating suggested in the Non-mandatory Appendix R, and you should see what is related to PWHT in this Code, which has some tables and graphs for this topic, in other words there is data that you have to take from your Building Code; Get advice from your Authorized ASME Inspector if you have a contract with an Authorized Inspection Agency.
Greetings!.

El sáb., 24 oct. 2020 a las 7:58, Jamie R (<jmerzr187@gmail.com>) escribió:
 your query is kind of broad. You should only involve the essential and non essential variables for each weld process used, stated in ASME Section IX. To involve ASME Sect. VIII without knowing what it is you are trying to incorporate, one would only be guessing. In short, there is no "essential requirements" when creating a weld procedure specification that you will find in a code of construction. Follow ASME IX and refer to the code of construction as needed.

On Friday, October 23, 2020 at 9:59:35 PM UTC-7 K K wrote:
Dear Experts,

Please refer below WPS and PQR details.

PQR Details - Base Metal - ASTM A106 Gr.B  To ASTM A106 Gr.B. ( P No - 1 Gr.No - 1 To  P No - 1 Gr.No - 1 ).
Process - GTAW  + SMAW ( GTAW - 4.8 mm + SMAW - 13.46 mm)
Thickness of the Coupon -18.26 mm, Dia - 6"
With PWHT - 638°C ,time 72 min.
No Impact tested.
DESIGN TEMP. / MDMT (°C) -290 / 5 .

WPS Details - Base Metal - ASTM A106 / A516 Gr.B / Gr.70  To  ASTM A106 / A516 Gr.B / Gr.70 . ( P No - 1 Gr.No - 1/2 To  P No - 1 Gr.No - 1/2 ).
Process - GTAW  + SMAW ( GTAW - 9.6 mm + SMAW - 15.4 mm).
SFA No- GTAW - 5.18 and for SMAW - 5.1.
AWS No - GTAW - ER70S-3 and SMAW - E7018-1H4R.
Pre heat - less than 12.7 mm -10°C and less than 25 mm 75°C.
Inter pass Temp. -315°C.
PWHT - 620°C, Holding time 1 hr thk +1 hour min.

According to above details help me to review, as per ASME Section VIII for Boiler and Pressure Vessel Code.
And I need your suggestion what are the essentials requirements according ASME  Sec.VIII. And what are the important things i have to check.
Please suggested me with clause reference.

Please send me your valuable suggestions, it's Supports me lot.

Thanks and Regards
Kiran




 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/517f0354-9d7e-46b1-9fb1-120a4c574fd5n%40googlegroups.com.


--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SUMMIT MÉXICO - TPI

https://www.linkedin.com/in/summit-m%C3%A9xico-tpi-760047137/

Móvil +52 1 812 352 4606

Skype: jjjimeneza





--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5ZurK_0KRhvs9gZJ66TDp3gnp1%3DrdwLeZT02%2BuCq4KwtP5WQ%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...