Wednesday, October 28, 2020

Re: [MW:31634] electrode selection

You can use E7018-1


From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> on behalf of QA/QC Deptt. TCPL <qc@tirupatisteel.com>
Sent: Wednesday, October 28, 2020 4:50:10 AM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:31632] electrode selection
 
Please suggest electrode for welding sa516 & sa105

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/96696980-d46c-4c18-a805-f06946c71e3en%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...