Hi, 

Did you noticed when constructing building the mason not keeping the brick one over another in same position. The first brick will start from corner, the second line will start by keeping the edge of brick at center of bottom one overlapping. No buildings bricks will be exactly one over another. Use this logic, to make sure the strength of the building. 

Similar way the longitudinal seam of one shell shall not be in same line as it weakens the joint. 


On Thu, 22 Oct 2020, 7:34 am Rajeev Shukla, <gkpshuklaji@gmail.com> wrote:
Sir

I need to under stand the meaning of this line , and which code I should refer for Compressor received welding.

Longitudinal seam in adjacent sections shall not be in same line.

On Saturday, 21 April 2018 at 11:57:35 UTC+5:30 joykol...@gmail.com wrote:
Dear Expert,

Please suggest Dia range.for WPS as per API 1104.

--



Best Regards,

Joydev Dalai
Dy. Manager - QA/QC
Kalpataru Power Transmission ltd.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c23d7c90-1f2b-4a58-ab4d-651cbde1c374n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALOPgmNjpSNUYOGEQZc4D4w8aB_cVg%2BKp7vSGZCn_XGLsBv__Q%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...