Hi,
There is no issue here, Root & Hot passes are essential variables at piping.
You can do.
On Thu, Oct 22, 2020 at 2:58 PM dorh <dorrihriz@gmail.com> wrote:
Hello ;
We work for welding activity pipeline 12" X52 thickness 8.38 mm
Root / hot pass GTAW
Filling / cap SMAW
In order to optimize production Contractor propose to proceed with GTAW first , for example for he weld first 10 weld joint GTAW after that he come back tomorrow with and filling and cap weld joint with SMAW.
It's some issue for that ?
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/386e7357-4115-479b-b8bf-45df08b78becn%40googlegroups.com.
With Regards
Udaya bahaskar.D
+919676270121
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3RM46AZv6-JgUUi4mZuJDTD%3DE5Ys7avJS-AKxOgvJo8BPg%40mail.gmail.com.