Hello,
PG will not cover 6G, Refer attached Welding positions.
Also need to change the Current , voltage according to Consumable Manufacturer Data sheet as per the thickness of electrodes. Then heat input <=3KJ/mm.
When preparing pWPS parameters need to consider as per data sheet of consumable.
Regards,
On Tue, Oct 20, 2020, 6:43 PM Hani Al Masry <hanyonalfy@gmail.com> wrote:
Dear Vinoth / Expertsi had prepared preliminary WPS as per ISO 15614-1 so please check all parameters and inputs are ok or notadditionally , check if this cover welding positions up to 6G and steel grade S355 and thickness up to 32mmAppreciate your fast action and assistanceRegards,H.A--On Sat, Oct 17, 2020 at 7:40 AM Hani Al Masry <hanyonalfy@gmail.com> wrote:how about· BS EN ISO 15614-1 Specification and qualification of welding procedures for metallic materials — Welding procedure test — Part 1: Arc and gas welding of steels and arc welding of nickel and nickel alloys
what is the major changes i need to made to the current WPS to convert it from AWS to
On Fri, Oct 16, 2020 at 7:29 AM Vinoth Rajendran <rajvinoth1987@gmail.com> wrote:Please go through EN ISO 15609, EN ISO 15614-1, EN ISO 9606--On Thu, Oct 15, 2020, 18:47 Hani Al Masry <hanyonalfy@gmail.com> wrote:Dear Experts--Our client is asking to convert our WPS from AWS to BS Standardscan you please advisewhich BS standards we need to usewhat the mean steps to be changed according to this BSRequirement of back stip for pipe weldingRegards,H.A
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKOkEzfjuGE1OGLGRz%2B7gY0syR5F8ifC9jRFWdyzzR3n7bZDXA%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2Ba0BHbLE%2BRtObsF4XaaMcen325c4QbBTeGs4DK5VDC%2ByeQV%2Bg%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKOkEzeQ36kA5njY74o4nv-c8QPGy7mmKGc4XywouR3mbmCFEg%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGQ515wG_%3DMQkEYDQDTVYdM8pW161EpHdbJ_p2MZzqUcDY8jBA%40mail.gmail.com.

Comments