Re: [MW:31634] electrode selection

E7018 SMAW
ER70S-6 GMAW / GTAW

El mié., 28 de octubre de 2020 1:55 a. m., QA/QC Deptt. TCPL <qc@tirupatisteel.com> escribió:
Please suggest electrode for welding sa516 & sa105

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/96696980-d46c-4c18-a805-f06946c71e3en%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5ZurKqiF_qrbUvU-oQQS7kG8f6pb5hOXiiFNuOehkL0tp4DA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...