Re: [MW:31656] PWHT Requirements

Greetings. Please specify the code of construction. If you would like an example, one could review ASME Section VIII Division 1; UW-40; UCS-56; Table UCS-56-1 for Post weld HeatTreatment Requirements of Carbon and Low Alloy Steels (P-No. 1)
Cheers.....
On Fri, Oct 30, 2020 at 11:55 PM Sujith Murali Issac <sujithms621@gmail.com> wrote:
ASME SEC VIII DIV 1 AND ASME SEC 1

On Sat, 31 Oct 2020 at 05:06, José Juan Jiménez Alejandro <jjjimeneza@gmail.com> wrote:
Construction Code?

El mié., 28 de octubre de 2020 11:40 p. m., Sujith Murali Issac <sujithms621@gmail.com> escribió:
Dear sirs,
  
        Please give me the requirements of the PWHT thickness ranges of Carbon steel materials

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5ade924c-7b40-4912-9adc-62dbf868df3dn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5ZurLe0i9hFK82DR%2BTXOz1q%2BRH-pajB5mD9GYuFVhmg%3DQE5g%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFbr%3DWGhM_Oci8LkhsjcmuUXxK3uzOvHuO4P0JMTpmgkZ2%3Dzrw%40mail.gmail.com.
--
Regards,
Jamie Reyes
J.R. Machine Company, Inc.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJNUtUPX9ys6%3DiB0k46THyaFpEFXp7rwg_dWPt5%2B-W_qG%2BHOQg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...