RE: [MW:31316] PWHT soak temperature variation

You can also verified microstructures of weldment, if its meet your requirement there is no issue.

 

Vimal Mistry I Tower SCM-QA

Mo#9099018064

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Vishwas Keskar
Sent: Monday, August 17, 2020 9:43 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:31308] PWHT soak temperature variation

 

CAUTION: External email. Do not click links or open attachments unless you recognize the sender and know the content is safe.
 

What is governing thickness 

Pl. calculate rate of heating as per ASME  SEC VIII 

It shall not be more than the calculated rate of heating

Steady Slope etc are not addressed.

 

 

No issue as per as weldment/parent material properties are concerned 

 

 

 

On Mon, Aug 17, 2020 at 7:33 AM Kandula Raju <rgkandula@gmail.com> wrote:

Dear Experts, 

 

   We have completed  post weld heat treatment of weld overlay in a large automatic programmer electrical furnace according to API6A and ASME Sec VIII Div.1, as per WPS heating rate shall be 100degree C per hour, so we have set heating rate from 300 to 600 degree C in 3 hours, however since its programme is computer controlled, we are reaching 100 degree C in 45 min instead of 1 hour and 15 min holding at each 100 degree progression, as per our customer heating rate shall have regular slope without any holding. Attached heat treatment chart for your review.

 

    Please do advice does it have any effect on weldment properties and is any code governs or states heating rate slope shall be steady.

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/F3571552-6D23-424A-8A72-996748F0EEE8%40gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3Pd-nJSg9ga11b2356EysLp9XnBzqPzv5XsfCXCRobeng%40mail.gmail.com.

------CONFIDENTIALITY NOTICE------- 
This email and any files transmitted with it are confidential and may be privileged or otherwise protected from disclosure under respective laws and are intended solely for the use of the entity / individual to whom they are addressed. If you have received this email in error or If you are not the intended recipient, please notify the sender immediately by way of telephone or email and delete this message and any files transmitted from your system. If you are not the intended recipient, you are hereby notified that any dissemination, distribution or copying of this communication is strictly prohibited. Please note that any views presented in the email are solely those of the author and do not necessarily represent those of the organization. While all care has been taken to avoid viruses the recipient is advised to check this email and attachments for presence of viruses. The organization accepts no liability on this account. We do not guarantee the security of any information transmitted through email and are not liable for any interception, corruption or delays. Anyone communicating with us by email accepts the risks of email communications and their consequences.
------CONFIDENTIALITY NOTICE-------

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...