[MW:31281] SS446 to SS446 (GTAW)

Dear Sirs,

Greetings !

We are in process to perform WPS/PQR for SS446 to SS446 combination.
Welding done on 20 mm thick plates using ER430 filler.

Test coupon passed for Tensile test but it is getting failed in Bend test .
Need your expertise opinions /suggestions  to complete this WPS/PQR with satisfactory results as per requirements of ASME Section IX .
Especially guidance  to pass Bend test .

Thanks in Advance

Regards
Prasad Loke

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3c8b9b28-f799-4ad7-a21e-d4a5d7e9c4b7o%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...