Tuesday, August 11, 2020

RE: [MW:31303] Change material grade of Nuts

In ASTM A194 – 2017, its Section 7.2 Also deleted.

But Still ASME Sec 2 (SA-194) latest edition have Grade 4.

 

Just for information

 

 

என்றும் அன்புடன்,
Thanks & Regards,

RAJAVARMAN
+971561895584

 

 

From: Dhanabal Jalachandran
Sent: 11 August 2020 07:57
To: materials-welding@googlegroups.com
Subject: Re: [MW:31302] Change material grade of Nuts

 

Dear,

 

Yes this statement was issued back in 2015 or 2016 edition of ASTM A 194, please refer the latest version under Section 7.2

 

Best Regards

 

DHANABAL JALACHANDRAN

Senior Inspector | Yanbu Steel Company

CSWIP 3.2.2 & BGAS Gr 2

 

Sent from Mail for Windows 10

 

On Mon, Aug 10, 2020 at 5:25 PM salim sogec <salimsogec84@gmail.com> wrote:

Dear Gents

 

Can we use ASTM A194 Grde-7 nus instead of ASTM A194 Grade-4nuts.

Because ASTM A194 Grade-4 nuts removed by the ASTM committee because globally lack of material availability.

 

Please advise.

Salim

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAH1-07WaQZ6VvLwZmwnf--t%3Dv5iBMmWuAigP1daFbF%2BKdHW%3D4g%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPLwtDfnqubdiqt1eM3_AVDQ4%2B0OPvTMznLcupThBhan2P%3Djwg%40mail.gmail.com.

 

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...