Dear all

Pls what is the current thickness requirements for PWHT as per ASME B31.3? 

I came across old version of the code, it specifies that PWHT not required for all P1 materials, provided min preheat is maintained at 95deg'C.

We intend welding; 18" sch 80(23.83mm) to ASTM A 106, 24" sch 80(30.8mm), is PWHT required? Cite relevant Code sections Please.

Regards,

Andrew. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAK1J--O6jttEt5bS1QCjykeCFnGeJpwoKsBqPPt9M_P1dOx%3DrA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...