[MW:31286] Ground flush on weld seam required at intersection location

Dear experts,

Generally, standards say that "The weld seam shall be ground flush for a distance 50 mm on all sides of the intersection".

What is exact technical reason to do for ground flush on weld seam required at intersection location?