I dont understand your question

Στις Τρί, 4 Αυγ 2020, 11:39 ο χρήστης 'Dinesh' via Materials & Welding <materials-welding@googlegroups.com> έγραψε:
Dear experts,
Please see the joint as below,

Here 4"x STD pipe welded with Nozzle #AY,CL150 4"x1" ( branch side thickness is 14 mm)

In as per project WPS,GTAW thickness range 12 mm Max and welder qualified range is 11.08 mm Max.
So in this branch ,how we can calculate thickness range (Like Governing thickness for PWHT) which accept or reject as per project requirement & B31.3 .

Thanks

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/af652036-0d04-4c79-aa1f-614dc6f73586n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40CsREzQ1w--%3DJ7tM%2Bj-S1BKpxWBD-SMWbcg1LAQkRZ5iw%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...