Re: [MW:31296] Combination of PQRs

Check the F-Numbers. If the are the same, then Check the A-Numbers. If they are also the same then you can go

Στις Σάβ, 1 Αυγ 2020, 14:20 ο χρήστης prasad loke <prasadloke27@gmail.com> έγραψε:
Dear Sir,
 
Greetings !
 
We are in need your expert opinion on following issue,
 
We have WPS/PQR for Incolloy 825-Incolloy 825 ( P number 45)----Filler used for same is from SFA 5.14
Now We have a requirement of SS904L to SS904L welding.( P number 45)---Where recommended filler is ER385 with SFA 5.9
 
If we make WPS with filler from SFA 5.14 for this (SS904L to SS904L) welding as P number is same, can it be supported with existing PQR of Inc-825 to INC-825 ?
 
Thanks in advance.
 
Regards
Prasad Loke

On Mon, Jul 27, 2020 at 1:03 PM K K <karan.hbl@gmail.com> wrote:

Hi Experts,


"Good Morning"


According to my line classes, I required NACE+HIC+PWHT Wet H2 services.

What is the test shall be conducted according to the standard to meet the requirements?


I have one PQR with NACE+PWHT+Wet H2S services, but not HIC test.

In addition, I have qualified one HIC tested PQR without PWHT no other lab test certificates, shall I combined this PQR to the above requirements( NACE+HIC+PWHT+wet H2S).

For your information, the HIC test is an additional requirement of our specifications.

Please looking your feedback on my above query.


Thanks and Regards

Kiran

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f1d53635-4e0f-4fe5-a0cf-ec93a8d2d87bo%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAS23S%2BpsvrtaQp%2B12MGvpjTP4jvPe5KrgK4JWyQXMjUabc1Lg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40AexAYUdPdWx7P0G3AoHwPQTb2rjJ%3DyBDiGvqcQ4kBdTg%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...