The minimum% NDT is governed by the applicable fluid service per ASME B31.3 Chapter VI.
The client can also request less stringent requirements, based on their own criteria and interests, this is totally valid, in the vast majority of countries the Code does not have legal implications, these criteria can be described in contracts, I mention it, since I am in a paper mill project, where most of the pipes carry water or water with pulp and therefore the interested company only requires 20% RT in the welded joints of the pipe systems. In other words, only some parts of the Code apply, it is only a reference, it is not mandatory in all its sections or parts.
The client can also request less stringent requirements, based on their own criteria and interests, this is totally valid, in the vast majority of countries the Code does not have legal implications, these criteria can be described in contracts, I mention it, since I am in a paper mill project, where most of the pipes carry water or water with pulp and therefore the interested company only requires 20% RT in the welded joints of the pipe systems. In other words, only some parts of the Code apply, it is only a reference, it is not mandatory in all its sections or parts.
El jue., 6 ago. 2020 a las 4:47, atul khatri (<atul.mnnit@gmail.com>) escribió:
Minimum NDT % is governed by applicable fluid service as per chapter VI of ASME B31.3.Client can always ask for more stringent requirements.I am attaching the NDT extent as per chapter VI for quick reference.Best regards,ATUL Khatri--On Aug 6, 2020 8:23 AM, "Mr. Sabi" <sabi2kg@gmail.com> wrote:It is based service and company procedure.--On Wed, Apr 11, 2018 at 2:53 PM Mukul <mukulhossen70@gmail.com> wrote:Dear Experts,--Can anybody help me by telling the RT percentage in ASME B31.3 ? Is the percentage is mentioned in the code or not ?Regards,Mukul Samad
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHma%3D444xNCDo1M_Wh3WsAeM1ys%3DNFKBnQo%3D_yN9i-A89CquDg%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACKOSeCtJr%2BfATbPr4sw_F_W%2BL6d3oyGNqhj3bo%2B7ZUU4m44wg%40mail.gmail.com.
Ing. José Juan Jiménez Alejandro
Independent Consultant in Parts
and Pressure Equipment
SUMMIT MÉXICO - TPI
https://www.linkedin.com/in/summit-m%C3%A9xico-tpi-760047137/
Móvil +52 1 812 352 4606
Skype: jjjimeneza
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5ZurLir2eqPJ60iminAjNq%3DwwG7wM8-EyT13f0wnmCrs_%2B4w%40mail.gmail.com.
Comments