Re: [MW:31308] PWHT soak temperature variation

What is governing thickness 
Pl. calculate rate of heating as per ASME  SEC VIII 
It shall not be more than the calculated rate of heating
Steady Slope etc are not addressed.


No issue as per as weldment/parent material properties are concerned 

 

On Mon, Aug 17, 2020 at 7:33 AM Kandula Raju <rgkandula@gmail.com> wrote:
Dear Experts, 

   We have completed  post weld heat treatment of weld overlay in a large automatic programmer electrical furnace according to API6A and ASME Sec VIII Div.1, as per WPS heating rate shall be 100degree C per hour, so we have set heating rate from 300 to 600 degree C in 3 hours, however since its programme is computer controlled, we are reaching 100 degree C in 45 min instead of 1 hour and 15 min holding at each 100 degree progression, as per our customer heating rate shall have regular slope without any holding. Attached heat treatment chart for your review.

    Please do advice does it have any effect on weldment properties and is any code governs or states heating rate slope shall be steady.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/F3571552-6D23-424A-8A72-996748F0EEE8%40gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3Pd-nJSg9ga11b2356EysLp9XnBzqPzv5XsfCXCRobeng%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...