IMHO I believe the reason for grinding this type of weld joint flush is for a good clear X-ray with no multiple beads showing on the film and no weave, Clear. Many years ago
when I worked as a welder for CBI / PDM / etc we always ground this type of joint flush because we always flat topped all the X-ray joints. The weld joints were not ground 'flush', 
they were 'flat topped', their is a difference. Flat topping a weld also gives a much clearer X-ray and it is faster than grinding joints flush. Also, I think tee joints could be called 
the 'weak link' in a weld, so to speak. I know of no code reference but that doesn't mean their isn't one.
Gene Matsko


On Thursday, August 6, 2020, 4:47:21 AM CDT, Sourav Bohrays <souravbohrays@gmail.com> wrote:


its a pleasure of mine if you show refference of this theory.
which code of construction you are using?

On Thu, 6 Aug 2020, 10:58 am 'Dinesh' via Materials & Welding, <materials-welding@googlegroups.com> wrote:
Dear experts,

Generally, standards say that "The weld seam shall be ground flush for a distance 50 mm on all sides of the intersection".

What is exact technical reason to do for ground flush on weld seam required at intersection location?

Inner side.jpg

Outer side.jpg

Thanks

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d734b305-0792-4fa6-aaf5-e06f2e75bb90n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOWr6k_NLJ2iQb3D16uuFJo8fTtDN%2BthoU-BtxN131TzJ1JY2Q%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...