Re: [MW:31310] Pre heating as per ASME SEC I / VIII DIV I

Preheating is determined by carbon equivalent value.

On Mon, Aug 17, 2020 at 08:26 Vishwas Keskar Welding Manager WELDING <vvkeskar123@gmail.com> wrote:

Specified thickness of the Pipe is 12.7 mm 
Actual thickness measured is 13mm 

Client specified preheating for  12.7 mm (=/>) =75 Deg C

Is preheating is to be decided on specified thickness or  actual thickness?
Any Construction Code back up >










--


https://materials-welding.blogspot.com/


https://www.linkedin.com/groups/122787


---


You received this message because you are subscribed to the Google Groups "Materials & Welding" group.


To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.


To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/23337554-0c50-46b4-911c-5fdac2322672n%40googlegroups.com.


--
THANKS AND REGARDS
CHRIS SABU
0559695451

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACY3QXQLbXQprp1m0xJZRqz-8ko0t3xqmrQuirXvei82QcJRHQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...