Never ,
selection for RT 100% not mean no hydro test , only for golden joint which for few case hydro test not possible.
what ever you need you have to cover by Clint specification and owner approval
Best regards
mahmoud
00201009087426
From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> on behalf of Mohan <ggnanamalli@gmail.com>
Sent: Wednesday, October 23, 2019 5:18 AM
To: materials-welding@googlegroups.com <materials-welding@googlegroups.com>
Subject: [MW:30175] Hydrotest of Pipings
Sent: Wednesday, October 23, 2019 5:18 AM
To: materials-welding@googlegroups.com <materials-welding@googlegroups.com>
Subject: [MW:30175] Hydrotest of Pipings
Dear Experts,
-- Kindly confirm whether we have did RT 100% -weld joints for the piping means no need of hydro-test.
If yes share the code reference.
Code of Construction : ASME B31.3
Regards
G Mohanraj
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEkUWtJG62wA-s8TVHu1peHGwu%2B%2BROMNm0HwewBwQPym56reZg%40mail.gmail.com.
Comments