Unable to understand exactly what are you looking for ?? U can refer Table -1 of SA336 /336 M . Austenitic steel grade F316 L is available .  SA-336 Grade F316L, ASME, SA-336/SA-336M, are Alloy Steel Forgings for Pressure and High-Temperature Parts. 

On Tue, 1 Oct 2019 at 14:15, Raghuram Bathula <raghurambathula@gmail.com> wrote:
it should have been SA965

On Tue, 1 Oct 2019 at 13:45, VIshal Suthar <vishalsuthar3017@gmail.com> wrote:
Dear Members,

Please note one of equipment client specification mentioned Tubesheet material SA 336 F 316L.

Reference to ASME Sec-II Part A SA336 is for Alloy Steel Forging which not having 316L.

Please provide your valued suggestion.

Regards,
VIshaL SUTHAR

-- 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubmOM3BA7xx8zqD6DNMs2nqT6E-yVLj%2BGJ1Nk9A%3DybcPkg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29OjvweKCJ%2ByiqcG-%3Ddk%2Brf1c636goV3X9SN9%2BjFYZUKXfw%40mail.gmail.com.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...