Re: [MW:30131] Distance between two weld joint

reference aramco standard w-11 
11.1
The minimum distance between parallel butt welds shall be 20 mm or 
three times the wall thickness of the joint, whichever is greater

On Wed, Oct 9, 2019, 10:32 AM Adam Janzeer <adamjanzeer4@gmail.com> wrote:
Dear moshin

Based on which reference....

On Wed, Oct 9, 2019 at 9:18 AM mohsin tufail <mohsin6tufail@gmail.com> wrote:
20mm or three times of the wall thickness which is greater

On Fri, Oct 4, 2019, 2:19 PM siva Guru <dhanaguru2010@gmail.com> wrote:
Dear All
Can you advice, 
two weld  joint how much Min distance between weldjoints.
Please clarify, if possible please provide code reference.

Best regards

Guru

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEDN%2BXFp1f7duhV4NFBmu_87QNzsuA877q4wDUTDuEOPTOM7eQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADa_Lup61kGNBO2ZjNA-K9sXC5ia-qZwmKsX1dNcYHwdVa6tzg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGKnWWjnnLYj%2B%3DnsHG-3SWmP3FYx0F8WXgbSNehb6iGEJLyi5g%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADa_Luqyf0gQx678fZWLzsJuVXSz2kq%2BAX6t6uxwX1cw7bgCaA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...