Dear Experts,

I would like to ask from all of you that i am working one of the project. I would like to confirm that butt welds with full penetration needs 100 percent radiographic test, is there any reference code? 
I have review the ISO 15614 code table 1 is about examination and testing of the test pieces should i consider this code to QIP.

Regards

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANOHF6tgMyhnE1vxz0iHWpwdynUFasYznL-2t62Smsmw5xpDaw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2Bh%3Dzr3QYCcmQUshWRf8P47Su93iLsTTOGZon1qcXezQOu7ibg%40mail.gmail.com.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...