Re: [MW:30176] Hydrotest of Pipings

Dear Sir,

Please see B31.3 Clause No.345.9 2016 Edition. Alternative Test of Leak Testing.

On Wed, Oct 23, 2019 at 10:58 AM Mohan <ggnanamalli@gmail.com> wrote:
Dear Experts,

Kindly confirm whether we have did RT 100% -weld joints for the piping means no need of hydro-test.
If yes share the code reference.

Code of Construction : ASME B31.3

Regards
G Mohanraj

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEkUWtJG62wA-s8TVHu1peHGwu%2B%2BROMNm0HwewBwQPym56reZg%40mail.gmail.com.


--
Thanks & Regard's


Kaushik Patel,
Surveyor,
Bureau Veritas - Gandhidham
Mobile: +91 9687000073.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJFrnNvFaZRyuNj1TOrfw%3D-J2ai1PknF70wnTUNm%3DHvw9wCATg%40mail.gmail.com.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...