[MW:30120] Re: materials

This is the general procedure followed by the industries to carry solution annealing for tubes after bending, no failure reported yet in my knowledge. There could be the possibility of sensitization in this area when you have high carbon ASS such as ASS304H in theory.



On Tuesday, October 1, 2019 at 11:15:37 AM UTC+3, kannayeram gnanapandithan wrote:
What is the difference between Reactive and Refractory Metals with example.

ASS 304-- Post bending heat treatment -Solution annealing was carried out for bent portion in Muffle furnace with straight portion projecting( around 2 mtrs) out. Is there any issue  in the transition area.

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4eb8894f-d76d-4d80-9e81-179c9b31c329%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...