Dear sir, 

If it's NABL approved lab in India,  may consider for approval. 

For EIL approved jobs, May not possible to approve. 

Applicable to Indian client works only. 

Regards

Dinesh

On Fri, Oct 18, 2019, 16:32 Santosh Patil <raj.san23@gmail.com> wrote:
Dear Members 


I have witnessed PQR of  SA312 TP 316 material 1" SCH 40  according to  Proposal WPS  , Test piece visually checked and send to Lab for check testing as per. Sec IX . also inform to vendor to be witness in Lab in the  presence of QC engineer . 
But vendor does not infirm to QC Engineer . and Lab test report is submitted . Now he pressurizes to approve WPS 
What shall I do..... 
S. B Patil

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAETO-3tBgdsVjUKbeb6BcAFMP%3DkuaPkErfTXe76vYDtxP_O%2BFw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAELgRrXjhfFL4PmvyOMf4uKJ10n%3Dt-6Ls%2Byg06%3DAnxk%2BQOyLhA%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...