Refer ASME Section IX, QW 407.1 as your dishend are single piece and will be normalized before welding. So you have to follow PWHT for qualification which is applicable after welding for your vessel.

On Monday, August 12, 2019 at 1:14:19 PM UTC+3, chiluka venkatramulu wrote:
Dear All,
Pl clarify the below.
One of vessel under fabrication will under go the fallowing heat treatments. (Material-516 G 70, shell-63 mm, dish end -75mm, dish end in one piece only)
  • Dishends Normalising-2 cycle.
  • PWHT for whole vessel.
Now shall I need to do all three heat treatment cycles to qualify WPS?
OR
Only two normalising cycles are enough?

Regards,
Venkatramulu

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6f573a01-0566-416e-99fa-248437a11066%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...