Sunday, October 6, 2019

[MW:30116] Re: Is PWHT required

As suggested by Jose the modification must be under R stamp,if u hv completed MDR & registered with NB.
Modification is possible as per customers requirements.Also PWHT after modifications may not be required if WPS/PQR is available.
 

On Wednesday, October 2, 2019 at 10:36:12 AM UTC+5:30, nvkkumar wrote:
Dear Gentleman,
We have received two vessels as per drawing. ASME U stamp done on both vessels, there is one bottom outlet nozzle of 6"NB in both vessels. Now client is asking us to remove the flange of the nozzle and hook up with piping. My doubt is 
1. Whether we have to take approval from authorized inspector before going to do any modification.
2. After hook up we have to do PWHT for that hook up joint
Please clarify, if possible please provide code reference.
Line SERVICE not call any PWHT
Construction code for vessel is ASME Sec VIII, Div 1, piping construction code is B 31.3.

Thanks in advance,


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0c2bc6bf-1f97-4013-b315-de40d9dc6c74%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...