Skip to main content

Re: [MW:30108] Re: PQR for PTAW Process by ASME Sec IX

Dear Sir
Construction code is API 6A

Kindly clarify below doubt, I have carried out trial welding on 25mm and 10mm test plate size of 170mmX170mm
1. I have carried out macro examination and no indication
2. Chemical analysis done at 1.6mm weld metal. Found Fe content in 10mm plate to 7.85% and 25mm plate 12.58%. Kindly clarify whether it is acceptable? do i need to check the chemical as per the filler wire composition? also normally dilution will not be controlled and Fe is observed above the spec

What is the acceptable limit?

3. As per the ASME Sec IX i have carried out 3 hardness at weld metal of 1.6mm as same as chemical test piece sample. Or do i need to check at the weld interface of weld metal, HAZ and base metal? kindly clarify

please give us the valuable inputs

On Wednesday, September 25, 2019 at 9:20:01 AM UTC+5:30, José Juan Jiménez Alejandro wrote:
It is important that you mention what the Construction Code is

El mar., 24 sept. 2019 a las 4:48, Bien_ND / weldinginspections.net (<bck...@gmail.com>) escribió:
please run follow machine manual and consumable manual.
I did a procedure PTA with Dura-Metal as them instruction.


On Monday, September 23, 2019 at 10:24:23 AM UTC+7, sathis...@gmail.com wrote:
> Dear Experts
>
> I would like to know below query on preparation of PQR as per ASME Sec IX, Process: PTAW by hardfacing overlay by Stellite 6 Powder
>
>
>
> 1. What is the current, voltage, Gas flow and Powder feed rate need to be maintained for 10mm and 25mm thickness plate. To which standard and reference i need to refer.
>
>
>
> 2. What is the pre heating and interpass temperature need to be maintained for P.No: 1,8,4,5A, 15E and to which standard need to refer
>
>
>
> 3. What is the hardness requirement for P.No: 1,8,4,5A, 15E during testing PQR? Which standard is mentioned this requirement?
>
>
>
> 4. Chemical analysis is mandatory for Co base as per ASME Sec IX , Table QW: 453
>
>
>
> Kindly give your suggestion and feedback for the above doubts
>
>
>
> Thanks in advance

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/26d6e35c-4e74-4687-a9b1-425343919b7e%40googlegroups.com.


--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SSI-TPI

Móvil +52 1 812 352 4606

Skype: jjjimeneza





--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/cb078006-4682-4287-96e8-754930c2aad5%40googlegroups.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...