Monday, October 7, 2019

Re: [MW:30120] Hot form dishead.

Thanks for valuable reply. 
If cold forming than pwht, hot forming normalized with ucs85. >5% , upto40%, 5% with any of five condition adressed pwht if cold formed, if hot formed normalizing with ucs85. That's it.. 

On Fri 4 Oct, 2019, 9:32 AM 'Prakash Hegde' via Materials & Welding, <materials-welding@googlegroups.com> wrote:
Hi
Code never address the temp.of hot forming
Generaly Hot forming is carried above Ac3 temp.i.e.about 900c and continue till say up to 850c This is judgment Till its plastcity is comfortable for forming
 In this case you may not require Post heat treatment as code has not addressed  This you may req to convince surveyor 

Second one is warm.forming say about 550 c It depends upon the configuration depth of DEnd also depends upon thk actual yield strength etc In this case Het treatment is essential after forming

Regards
Hegde




On Fri, 4 Oct 2019 at 8:37, Souravbohray
hi i need some info as per experience and asme sec8 div1..
1.if dishead is cold form and fe >5% than pwht to be done ucs 79
2.if pwht required for vessel fe can be upto40% ucs79
3.if fe>5% and dish head is hot formed ...
Q-1. Is it compulsory that hot forming should be done at temprature above lower critical temprature?
Q-2 if temprature is more than 480 than normalizing to be done for hot forming dish head with ucs 85 simulation test coupon?
Q-3 at what thickness hot forming, cold forming to be done dnt use the Eil specification?
Q-4 if dish head is hot formed fe>5% than also only pwht to be done as per ucs 79

--
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/FY-U45g81QA/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1029307210.2962912.1570161191047%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALGgjPWeasQzgGicSp-LU6kWVPErxpuEOzG7xUme%2B0VGA%3DFWyA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...