[MW:30162] WPS /PQR Approvel

Dear Members 


I have witnessed PQR of  SA312 TP 316 material 1" SCH 40  according to  Proposal WPS  , Test piece visually checked and send to Lab for check testing as per. Sec IX . also inform to vendor to be witness in Lab in the  presence of QC engineer . 
But vendor does not infirm to QC Engineer . and Lab test report is submitted . Now he pressurizes to approve WPS 
What shall I do..... 
S. B Patil

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAETO-3tBgdsVjUKbeb6BcAFMP%3DkuaPkErfTXe76vYDtxP_O%2BFw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...